Technical Data | Zirconia Corundum Mullite Brick | |
CMZ-6 | ||
Chemical Composition (wt%) | Al2O3 | ≥87 |
ZrO2 | ≥6 | |
SiO2 | ≤4 | |
Volume Density (kg/m3) | ≥3000 | |
Apparent Porosity (%) | ≤18 | |
Normal Temperature Compression Strength (MPa) | ≥100 | |
Refractoriness under Load (℃) | 0.2MPa,0.6% | >1700 |
Refiring Linear Change (%) | 1600℃×3h | ±0.2 |
Thermal Shock Stability (Times) | 1100℃×20min,water-cooling | ≥30 |